The present invention relates to a manufacturing method of eco-friendly yellow soil mortar and a construction method of yellow soil mortar, and more specifically, to a manufacturing method of eco-friendly yellow soil mortar which has functionality such as a far-infrared radiation, which is helpful to a human body, a negative ion, deodorization, antibacterial function, etc. by using yellow soil as a main material, and is excellent in keeping warmth and insulation in order not to generate a crack after construction. According to the present invention, the manufacturing method of eco-friendly yellow soil mortar comprises: a ripening step of ripening collected yellow soil for three years; a drying step of drying the yellow soil, passed through the ripening step, in a place where sunlight is blocked; a selection step of filtering the yellow soil, passed through the drying step, with three meshes; a grinding step of grinding the yellow soil, passed through the selection step, in a size of 325 to 600 mesh; and a mixing and stirring step of mixing 92 to 95 weight% of yellow soil powder passed through the grinding step, 4 to 6 weight% of regenerated pulp powder, and 1 to 2 weight% of white cement, and stirring for 10 to 15 minutes.
본 발명은 친환경 황토 모르타르 제조방법 및 황토 모르타르 시공방법에 관한 것으로, 보다 상세하게는 황토를 주원료로 하여 인체에 유익한 원적외선, 음이온 및 탈취, 항균 등의 기능성을 발휘함은 물론 보온 및 단열 효과가 우수하며, 시공 후 균열이 발생되지 않도록 한 친환경 황토 모르타르 제조방법 및 황토 모르타르 시공방법에 관한 것이다. 본 발명에 따른 친환경 황토 모르타르 제조방법은, 채집된 황토를 3년간 숙성시키는 숙성단계와; 상기 숙성단계를 거친 황토를 햇빛이 차단된 장소에서 건조시키는 건조단계와; 상기 건조단계를 거친 황토를 3메쉬로 체거름하는 선별단계와; 상기 선별단계를 거친 황토를 325~600메쉬 크기로 분쇄시키는 분쇄단계와; 상기 분쇄단계를 거친 황토분말 92~95 중량%와, 재생펄프 분말 4~6 중량%와, 백시멘트 1~2 중량%를 혼합용기에서 혼합하고 10~15분간 교반시키는 혼합교반단계를 포함하는 것을 특징으로 한다.
The present invention relates to a manufacturing method of eco-friendly yellow soil mortar and a construction method of yellow soil mortar, and more specifically, to a manufacturing method of eco-friendly yellow soil mortar which has functionality such as a far-infrared radiation, which is helpful to a human body, a negative ion, deodorization, antibacterial function, etc. by using yellow soil as a main material, and is excellent in keeping warmth and insulation in order not to generate a crack after construction. According to the present invention, the manufacturing method of eco-friendly yellow soil mortar comprises: a ripening step of ripening collected yellow soil for three years; a drying step of drying the yellow soil, passed through the ripening step, in a place where sunlight is blocked; a selection step of filtering the yellow soil, passed through the drying step, with three meshes; a grinding step of grinding the yellow soil, passed through the selection step, in a size of 325 to 600 mesh; and a mixing and stirring step of mixing 92 to 95 weight% of yellow soil powder passed through the grinding step, 4 to 6 weight% of regenerated pulp powder, and 1 to 2 weight% of white cement, and stirring for 10 to 15 minutes.
본 발명은 친환경 황토 모르타르 제조방법 및 황토 모르타르 시공방법에 관한 것으로, 보다 상세하게는 황토를 주원료로 하여 인체에 유익한 원적외선, 음이온 및 탈취, 항균 등의 기능성을 발휘함은 물론 보온 및 단열 효과가 우수하며, 시공 후 균열이 발생되지 않도록 한 친환경 황토 모르타르 제조방법 및 황토 모르타르 시공방법에 관한 것이다. 본 발명에 따른 친환경 황토 모르타르 제조방법은, 채집된 황토를 3년간 숙성시키는 숙성단계와; 상기 숙성단계를 거친 황토를 햇빛이 차단된 장소에서 건조시키는 건조단계와; 상기 건조단계를 거친 황토를 3메쉬로 체거름하는 선별단계와; 상기 선별단계를 거친 황토를 325~600메쉬 크기로 분쇄시키는 분쇄단계와; 상기 분쇄단계를 거친 황토분말 92~95 중량%와, 재생펄프 분말 4~6 중량%와, 백시멘트 1~2 중량%를 혼합용기에서 혼합하고 10~15분간 교반시키는 혼합교반단계를 포함하는 것을 특징으로 한다.
METHOD FOR MANUFACTURING OF ECO-FRIENDLY YELLOW SOIL MORTAR AND METHOD FOR CONSTRUCTING OF YELLOW SOIL MORTAR
친환경 황토 모르타르 제조방법 및 황토 모르타르 시공방법
JO IN OK (author)
2015-05-29
Patent
Electronic Resource
Korean
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|Compositon for yellow soil mortar and yellow soil board using the same
European Patent Office | 2021
|Method for manufacturing environment-friendly yellow soil board
European Patent Office | 2018
|