Disclosed are a waterproof asphalt concrete additive, a manufacturing method thereof, waterproof asphalt concrete, a manufacturing method thereof, and a waterproof asphalt concrete construction method. The manufacturing method of waterproof asphalt concrete additive comprises the following steps of: heating a basic additive which is obtained by selecting two or more among silica sand, rubber powder, and calcium carbonate having a diameter less than or equal to 0.67 mm, and by mixing the same; adding a process oil to SBS and preparing aged SBS by aging the SBS for one hour or more to add the aged SBS to the basic additive; further adding Bron asphalt to the basic additive; preparing a primary additive by selecting any one among calcium carbonate, cement, and slaked lime and further adding the same to the basic additive; cooling the primary additive; and adding a secondary additive including the aged SBS to the cooled primary additive, and mixing the same.
방수 아스콘 첨가제 및 그 제조방법, 방수 아스콘 및 그 제조방법 그리고, 방수 아스콘 시공방법이 소개된다. 본 발명의 방수 아스콘 첨가제 제조방법은, 0.67mm 이하의 규사, 고무분말, 탄산칼슘 중 2개 이상을 선택하여 혼합한 기초 첨가제를 가열하는 과정; SBS에 프로세스오일을 첨가하고, 1시간 이상 숙성시켜 숙성 SBS를 제조하여 상기 숙성 SBS를 상기 기초 첨가제에 첨가하는 과정; 상기 기초 첨가제에 브론 아스팔트를 더 첨가하는 과정; 탄산칼슘, 시멘트, 소석회 중 어느 하나를 선택하여 상기 기초 첨가제에 더 첨가하여 1차 첨가제를 제조하는 과정; 상기 1차 첨가제를 냉각시키는 과정; 및 냉각된 상기 1차 첨가제에 숙성 SBS를 포함하는 2차 첨가제를 더 첨가하여 혼합하는 과정을 포함한다.
Waterproof Ascon agent and its manufacturing method waterproof Ascon and its manufacturing method and waterproof Ascon construction method
Disclosed are a waterproof asphalt concrete additive, a manufacturing method thereof, waterproof asphalt concrete, a manufacturing method thereof, and a waterproof asphalt concrete construction method. The manufacturing method of waterproof asphalt concrete additive comprises the following steps of: heating a basic additive which is obtained by selecting two or more among silica sand, rubber powder, and calcium carbonate having a diameter less than or equal to 0.67 mm, and by mixing the same; adding a process oil to SBS and preparing aged SBS by aging the SBS for one hour or more to add the aged SBS to the basic additive; further adding Bron asphalt to the basic additive; preparing a primary additive by selecting any one among calcium carbonate, cement, and slaked lime and further adding the same to the basic additive; cooling the primary additive; and adding a secondary additive including the aged SBS to the cooled primary additive, and mixing the same.
방수 아스콘 첨가제 및 그 제조방법, 방수 아스콘 및 그 제조방법 그리고, 방수 아스콘 시공방법이 소개된다. 본 발명의 방수 아스콘 첨가제 제조방법은, 0.67mm 이하의 규사, 고무분말, 탄산칼슘 중 2개 이상을 선택하여 혼합한 기초 첨가제를 가열하는 과정; SBS에 프로세스오일을 첨가하고, 1시간 이상 숙성시켜 숙성 SBS를 제조하여 상기 숙성 SBS를 상기 기초 첨가제에 첨가하는 과정; 상기 기초 첨가제에 브론 아스팔트를 더 첨가하는 과정; 탄산칼슘, 시멘트, 소석회 중 어느 하나를 선택하여 상기 기초 첨가제에 더 첨가하여 1차 첨가제를 제조하는 과정; 상기 1차 첨가제를 냉각시키는 과정; 및 냉각된 상기 1차 첨가제에 숙성 SBS를 포함하는 2차 첨가제를 더 첨가하여 혼합하는 과정을 포함한다.
Waterproof Ascon agent and its manufacturing method waterproof Ascon and its manufacturing method and waterproof Ascon construction method
방수 아스콘 첨가제 및 그 제조방법, 방수 아스콘 및 그 제조방법 그리고, 방수 아스콘 시공방법
HWANG IK HYUN (author) / HWANG JU CHUL (author)
2019-05-07
Patent
Electronic Resource
Korean
European Patent Office | 2019