WEAK FOUNDATION TREATMENT METHOD
The present invention relates to a weak ground rapid-treatment method and, more specifically, to a weak ground rapid-treatment method which can be used with a minimum number of curing conditions for weak ground solidification treatment construction in urgent construction or winter construction with low temperature through hardening-promotion and anti-freezing functions by byproducts containing chlorine components. In accordance with the present invention, the weak ground rapid-treatment method includes: 1) installing an injection pipe in the ground; 2) mixing a ground solidification material with water to produce a ground grouting material; 3) transferring and injecting the ground grouting material through the injection pipe; and 4) curing the ground grouting material by hardening the same. The ground solidification material, with respect to 100 parts by weight of blast furnace slag powder of which the specific surface area is 4,000-8,000 cm2/g, includes: 0.5-1,000 parts by weight of bottom ash of a circulating fluidized bed boiler having a particle size adjusted to no more than 0.1-5 mm, having a CaO content of 15-70 wt% and an SO3 content of 3-35 wt%; 0.5-500 parts by weight of ironworks sodium bicarbonate desulfurization dust having a chlorine content of 1-20 wt%; 0.5-500 parts by weight of ironworks lime desulfurization dust having a chlorine content of 0.5-10 wt%; 0.5-500 parts by weight of a solid fuel combustion material having a chlorine content of 0.1-10 wt%; and 5-300 parts by weight of cement.
본 발명은 연약지반 급속 처리방법에 관한 것으로서, 보다 상세하게는 염소 성분을 함유한 부산물에 의한 경화 촉진 및 동결방지 기능에 의해 기온이 낮은 겨울철 공사나 긴급한 공사의 연약 지반 고화 처리 공사시 최소한의 양생 조건을 갖추고 사용할 수 있는 연약지반 급속 처리방법에 관한 것이다. 본 발명에 의한 연약지반 급속 처리방법은 1) 지반에 주입관을 설치하는 단계; 2) 지반 고화재를 물과 혼합하여 지반 그라우팅재를 제조하는 단계; 3) 상기 지반 그라우팅재를 상기 주입관을 통해 이송하여 주입시키는 단계; 및 4) 상기 지반 그라우팅재를 경화시켜 양생하는 단계;를 포함하며, 상기 지반 고화재는, 비표면적이 4,000∼8,000cm2/g인 고로슬래그 미분말 100중량부에 대하여, 0.1∼5mm로 이하로 입도가 조정되고 CaO 함량이 15∼70중량%이고 SO3 함량이 3∼35중량%인 순환 유동층 보일러 바텀애시 0.5∼1,000중량부와, 염소 함유량이 1∼20중량%인 제철소 중조 탈황 분진 0.5∼500중량부와, 염소 함유량이 0.5∼10중량%인 제철소 석회 탈황 분진 0.5∼500중량부와, 염소 함유량이 0.1∼10중량%인 고형연료 연소재 0.5∼500중량부와, 시멘트 5∼300중량부를 포함하는 것을 특징으로 한다.
WEAK FOUNDATION TREATMENT METHOD
The present invention relates to a weak ground rapid-treatment method and, more specifically, to a weak ground rapid-treatment method which can be used with a minimum number of curing conditions for weak ground solidification treatment construction in urgent construction or winter construction with low temperature through hardening-promotion and anti-freezing functions by byproducts containing chlorine components. In accordance with the present invention, the weak ground rapid-treatment method includes: 1) installing an injection pipe in the ground; 2) mixing a ground solidification material with water to produce a ground grouting material; 3) transferring and injecting the ground grouting material through the injection pipe; and 4) curing the ground grouting material by hardening the same. The ground solidification material, with respect to 100 parts by weight of blast furnace slag powder of which the specific surface area is 4,000-8,000 cm2/g, includes: 0.5-1,000 parts by weight of bottom ash of a circulating fluidized bed boiler having a particle size adjusted to no more than 0.1-5 mm, having a CaO content of 15-70 wt% and an SO3 content of 3-35 wt%; 0.5-500 parts by weight of ironworks sodium bicarbonate desulfurization dust having a chlorine content of 1-20 wt%; 0.5-500 parts by weight of ironworks lime desulfurization dust having a chlorine content of 0.5-10 wt%; 0.5-500 parts by weight of a solid fuel combustion material having a chlorine content of 0.1-10 wt%; and 5-300 parts by weight of cement.
본 발명은 연약지반 급속 처리방법에 관한 것으로서, 보다 상세하게는 염소 성분을 함유한 부산물에 의한 경화 촉진 및 동결방지 기능에 의해 기온이 낮은 겨울철 공사나 긴급한 공사의 연약 지반 고화 처리 공사시 최소한의 양생 조건을 갖추고 사용할 수 있는 연약지반 급속 처리방법에 관한 것이다. 본 발명에 의한 연약지반 급속 처리방법은 1) 지반에 주입관을 설치하는 단계; 2) 지반 고화재를 물과 혼합하여 지반 그라우팅재를 제조하는 단계; 3) 상기 지반 그라우팅재를 상기 주입관을 통해 이송하여 주입시키는 단계; 및 4) 상기 지반 그라우팅재를 경화시켜 양생하는 단계;를 포함하며, 상기 지반 고화재는, 비표면적이 4,000∼8,000cm2/g인 고로슬래그 미분말 100중량부에 대하여, 0.1∼5mm로 이하로 입도가 조정되고 CaO 함량이 15∼70중량%이고 SO3 함량이 3∼35중량%인 순환 유동층 보일러 바텀애시 0.5∼1,000중량부와, 염소 함유량이 1∼20중량%인 제철소 중조 탈황 분진 0.5∼500중량부와, 염소 함유량이 0.5∼10중량%인 제철소 석회 탈황 분진 0.5∼500중량부와, 염소 함유량이 0.1∼10중량%인 고형연료 연소재 0.5∼500중량부와, 시멘트 5∼300중량부를 포함하는 것을 특징으로 한다.
WEAK FOUNDATION TREATMENT METHOD
연약지반 급속 처리방법
LIM YANG HYUN (author) / SEO SE GWAN (author) / AN YANG JIN (author) / MUN GYOUNG JU (author)
2021-06-16
Patent
Electronic Resource
Korean
FOUNDATION TREATMENT METHOD FOR WEAK HYDRAULIC-FILL REGION
European Patent Office | 2022
|European Patent Office | 2023
|Weak geological building foundation reinforcement construction method
European Patent Office | 2021
|