Effects of Isothermal Aging on the Microstructure and Tensile Behavior of Sn-3.0Ag-0.5Cu-0.2Co Solder
Effects of Isothermal Aging on the Microstructure and Tensile Behavior of Sn-3.0Ag-0.5Cu-0.2Co Solder
Effects of Isothermal Aging on the Microstructure and Tensile Behavior of Sn-3.0Ag-0.5Cu-0.2Co Solder
Cheng, F.J. (Autor:in) / Nishikawa, H. (Autor:in) / Takemoto, T. (Autor:in) / Lee, C. / Lee, J.-B. / Park, D.-H. / Na, S.-J.
01.01.2008
4 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Fracture of sustained tensile-loaded Sn-3.0Ag-0.5Cu solder alloy in NaCl solution
British Library Online Contents | 2011
|Hardness profiles of Sn-3.0Ag-0.5Cu-TiO2 composite solder by nanoindentation
British Library Online Contents | 2016
|Hardness profiles of Sn-3.0Ag-0.5Cu-TiO2 composite solder by nanoindentation
British Library Online Contents | 2016
|British Library Online Contents | 2014
|