Deuterium concentration depth profiling in sputter-deposited tungsten coated F82H using secondary ion mass spectrometry
Deuterium plasma-driven permeation (PDP) through reduced activation ferritic steel alloy F82H with and without sputter-deposited tungsten (SP-W) coatings has been conducted using a laboratory-scale steady-state plasma facility. SP-W coatings have been found to enhance PDP flux with a much slow breakthrough to reach steady-state. Static deuterium retention has been evaluated with thermal desorption spectroscopy. Enhanced deuterium retention in SP-W coated F82H has been observed, compared with that in bare F82H. Secondary ion mass spectrometry (SIMS) has been carried out to obtain the depth profile of deuterium concentration crossing the W/F82H interface. SIMS data indicate the deuterium concentration is much higher in W coatings than that in F82H substrate, exhibiting an “uphill diffusion” profile. Keywords: Plasma-driven permeation, SIMS, Tungsten coatings, F82H, Deuterium retention
Deuterium concentration depth profiling in sputter-deposited tungsten coated F82H using secondary ion mass spectrometry
Deuterium plasma-driven permeation (PDP) through reduced activation ferritic steel alloy F82H with and without sputter-deposited tungsten (SP-W) coatings has been conducted using a laboratory-scale steady-state plasma facility. SP-W coatings have been found to enhance PDP flux with a much slow breakthrough to reach steady-state. Static deuterium retention has been evaluated with thermal desorption spectroscopy. Enhanced deuterium retention in SP-W coated F82H has been observed, compared with that in bare F82H. Secondary ion mass spectrometry (SIMS) has been carried out to obtain the depth profile of deuterium concentration crossing the W/F82H interface. SIMS data indicate the deuterium concentration is much higher in W coatings than that in F82H substrate, exhibiting an “uphill diffusion” profile. Keywords: Plasma-driven permeation, SIMS, Tungsten coatings, F82H, Deuterium retention
Deuterium concentration depth profiling in sputter-deposited tungsten coated F82H using secondary ion mass spectrometry
Y. Xu (Autor:in) / Y. Hirooka (Autor:in) / L.M. Luo (Autor:in) / Y.C. Wu (Autor:in)
2019
Aufsatz (Zeitschrift)
Elektronische Ressource
Unbekannt
Metadata by DOAJ is licensed under CC BY-SA 1.0
Sputter depth profiling by secondary ion mass spectrometry coupled with sample current measurements
British Library Online Contents | 2006
|Springer Verlag | 1992
|Depth profiling using ultra-low-energy secondary ion mass spectrometry
British Library Online Contents | 2003
|Method for sputter rate determination in sputter depth profiling
British Library Online Contents | 1993
|Method for sputter rate determination in sputter depth profiling
British Library Online Contents | 1993
|