High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere
A high-strength geopolymer hollow microsphere, a preparation method thereof and a phase change energy storage microsphere are provided, including: dissolving sodium hydroxide, sodium silicate and spheroidizing aid in water to form a solution A, and adding active powder to the solution A, stirring and uniformly mixing to form a slurry B, adding the slurry B to an oil phase, stirring and dispersing into balls, filtering to obtain geopolymer microspheres I, washing the geopolymer microspheres I, and then carrying out a high-temperature calcination to obtain the high-strength geopolymer hollow microspheres II; using the high-strength geopolymer hollow microsphere as a carrier, absorbing a phase change material into the carrier, and mixing a microsphere carrying the phase change material with an epoxy resin, adding a powder dispersant and stirring to disperse the microsphere, after the epoxy resin is solidified, screening the superfluous powder dispersant to obtain the phase energy storage microsphere.
High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere
A high-strength geopolymer hollow microsphere, a preparation method thereof and a phase change energy storage microsphere are provided, including: dissolving sodium hydroxide, sodium silicate and spheroidizing aid in water to form a solution A, and adding active powder to the solution A, stirring and uniformly mixing to form a slurry B, adding the slurry B to an oil phase, stirring and dispersing into balls, filtering to obtain geopolymer microspheres I, washing the geopolymer microspheres I, and then carrying out a high-temperature calcination to obtain the high-strength geopolymer hollow microspheres II; using the high-strength geopolymer hollow microsphere as a carrier, absorbing a phase change material into the carrier, and mixing a microsphere carrying the phase change material with an epoxy resin, adding a powder dispersant and stirring to disperse the microsphere, after the epoxy resin is solidified, screening the superfluous powder dispersant to obtain the phase energy storage microsphere.
High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere
LIU HUAJIE (Autor:in) / BU YUHUAN (Autor:in) / MA RUI (Autor:in) / GUO SHENGLAI (Autor:in) / AN LONGLONG (Autor:in)
27.06.2023
Patent
Elektronische Ressource
Englisch
Europäisches Patentamt | 2023
|High-strength ceramic microsphere and preparation method thereof
Europäisches Patentamt | 2021
|Low-cost hollow silicon carbide microsphere and preparation method thereof
Europäisches Patentamt | 2023
|Ceramic hollow microsphere as well as preparation method and application thereof
Europäisches Patentamt | 2023
|