The invention discloses a manufacturing method of imitation Sanpu mountain gneissic granite stone line ceramic. The method is easy to operate, and during the firing process, kiln transformation occurs on an enamel layer to form the imitation Sanpu mountain gneissic granite stone line ceramic. The method comprises the steps that chromophore materials containing stannic dioxide, zirconium dioxide, nickel oxide, cobaltous oxide, chromic oxide, ferric oxide, manganese dioxide and antimony oxide are prepared, glaze slip with 45-52 wt% of total solid content is prepared by being mixed with transparent basic glaze, and firing is conducted on a glazed ceramic body to obtain an imitation Sanpu mountian gneissic granite stone line ceramic product. According to the manufacturing method of the imitation Sanpu mountian gneissic granite stone line ceramic, the kiln transformation occurs on the enamel layer during the firing process, color spots with colors such as ash black and white appear on the enamel layer of a fired ceramic product, the shade and the distribution state of the color spots are similar to Sanpu mountain gneissic granite, and the visual effect of the appearance of the Sanpu mountain gneissic granite is achieved. Glazing in one time is adopted, the labor cost is greatly reduced, and the production efficiency is improved.
Manufacturing method of imitation Sanpu mountain gneissic granite stone line ceramic
The invention discloses a manufacturing method of imitation Sanpu mountain gneissic granite stone line ceramic. The method is easy to operate, and during the firing process, kiln transformation occurs on an enamel layer to form the imitation Sanpu mountain gneissic granite stone line ceramic. The method comprises the steps that chromophore materials containing stannic dioxide, zirconium dioxide, nickel oxide, cobaltous oxide, chromic oxide, ferric oxide, manganese dioxide and antimony oxide are prepared, glaze slip with 45-52 wt% of total solid content is prepared by being mixed with transparent basic glaze, and firing is conducted on a glazed ceramic body to obtain an imitation Sanpu mountian gneissic granite stone line ceramic product. According to the manufacturing method of the imitation Sanpu mountian gneissic granite stone line ceramic, the kiln transformation occurs on the enamel layer during the firing process, color spots with colors such as ash black and white appear on the enamel layer of a fired ceramic product, the shade and the distribution state of the color spots are similar to Sanpu mountain gneissic granite, and the visual effect of the appearance of the Sanpu mountain gneissic granite is achieved. Glazing in one time is adopted, the labor cost is greatly reduced, and the production efficiency is improved.
Manufacturing method of imitation Sanpu mountain gneissic granite stone line ceramic
CHEN SHUBO (author) / CHEN PEIJUAN (author) / CHEN XIAOXIANG (author) / SU XIAOJIE (author) / CHEN XIAOHUI (author) / CAI QINGLIN (author)
2015-11-11
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Manufacturing method for imitative Sangpu mountain gneissic granite concave-convex anilox ceramic
European Patent Office | 2015
|Manufacturing method of imitation India red stone line ceramic
European Patent Office | 2015
|Granite ceramic tile with natural stone texture and manufacturing method thereof
European Patent Office | 2021
|