Polymer repair mortar and preparation method thereof
The invention relates to the technical field of repair mortar, in particular to polymer repair mortar and a preparation method thereof. The polymer repair mortar comprises the following components inparts by mass: 100 parts of Portland cement, 150 to 160 parts of talcum powder, 30 to 35 parts of zeolite powder, 30 to 35 parts of calcite powder, 40 to 45 parts of marble powder, 40 to 45 parts of dolomite dust, 30 to 35 parts of fluorite powder, 20 to 25 parts of zircon powder, 20 to 25 parts of hexacyclic stone powder, 3 to 5 parts of trimethylphenylselenosilane; 0.2 to 0.3 parts of fifurazone, and 90-100 parts of water. The polymer repair mortar has the effect that a crack repaired through the polymer repair mortar is high in freezing resistance, stable in structure and not prone to cracking again.
本发明涉及修补砂浆的技术领域,具体涉及一种聚合物修补砂浆及其制备方法,其包括以下质量份数的组分:硅酸盐水泥100份;滑石粉150‑160份;沸石粉30‑35份;方解石粉30‑35份;大理石粉40‑45份;白云石粉40‑45份;萤石粉30‑35份;锆石粉20‑25份;六环石粉20‑25份;三甲基苯基硒硅烷3‑5份;硝呋烯腙0.2‑0.3份;水90‑100份。本发明具有通过聚合物修补砂浆修补后的裂缝处抗冻能力较强,结构稳定,不易再次开裂的效果。
Polymer repair mortar and preparation method thereof
The invention relates to the technical field of repair mortar, in particular to polymer repair mortar and a preparation method thereof. The polymer repair mortar comprises the following components inparts by mass: 100 parts of Portland cement, 150 to 160 parts of talcum powder, 30 to 35 parts of zeolite powder, 30 to 35 parts of calcite powder, 40 to 45 parts of marble powder, 40 to 45 parts of dolomite dust, 30 to 35 parts of fluorite powder, 20 to 25 parts of zircon powder, 20 to 25 parts of hexacyclic stone powder, 3 to 5 parts of trimethylphenylselenosilane; 0.2 to 0.3 parts of fifurazone, and 90-100 parts of water. The polymer repair mortar has the effect that a crack repaired through the polymer repair mortar is high in freezing resistance, stable in structure and not prone to cracking again.
本发明涉及修补砂浆的技术领域,具体涉及一种聚合物修补砂浆及其制备方法,其包括以下质量份数的组分:硅酸盐水泥100份;滑石粉150‑160份;沸石粉30‑35份;方解石粉30‑35份;大理石粉40‑45份;白云石粉40‑45份;萤石粉30‑35份;锆石粉20‑25份;六环石粉20‑25份;三甲基苯基硒硅烷3‑5份;硝呋烯腙0.2‑0.3份;水90‑100份。本发明具有通过聚合物修补砂浆修补后的裂缝处抗冻能力较强,结构稳定,不易再次开裂的效果。
Polymer repair mortar and preparation method thereof
聚合物修补砂浆及其制备方法
LIAO XIAOBO (author)
2020-05-29
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Anti-aging polymer repair mortar and preparation method thereof
European Patent Office | 2024
|Multifunctional inorganic polymer repair mortar and preparation method thereof
European Patent Office | 2020
|Polymer reinforced fiber modified repair mortar and preparation method thereof
European Patent Office | 2021
|Polymer repair mortar for marine concrete and preparation method thereof
European Patent Office | 2024
|