A platform for research: civil engineering, architecture and urbanism
The invention relates to the field of concrete interface agents, and particularly discloses a freeze-thaw resistant breathable concrete interface agent. The interface agent is prepared from the following raw materials in parts by weight: 50 to 100 parts of ordinary Portland cement, 10 to 20 parts of sulphoaluminate cement, 10 to 20 parts of gypsum, 10 to 20 parts of silica fume, 10 to 20 parts offly ash, 50 to 100 parts of PTB emulsion, 10 to 15 parts of waterborne acrylate laminating adhesive, 5 to 10 parts of bamboo liquefied phenolic resin, 1 to 2 parts of an air entraining agent, 1 to 2 parts of dispersant, 0.5 to 1 part of a foam breaker and 100 to 200 parts of water. The interface agent can be applied to binding new and old concrete, and has the advantages of high bonding strength,high freeze-thaw resistance and high air permeability.
本申请涉及混凝土界面剂领域,具体公开了一种抗冻融型透气混凝土界面剂。按重量份计,所述界面剂原料包括普通硅酸盐水泥50~100份,硫铝酸盐水泥10~20份,石膏10~20份,微硅粉10~20份,粉煤灰10~20份,PTB乳液50~100份,水性丙烯酸酯复膜胶10~15份,竹材液化酚醛树脂5~10份,引气剂1~2份,分散剂1~2份,消泡剂0.5~1份,水100~200份,本申请的界面剂可用于粘结新老混凝土,其具有粘结强度高、抗冻融性好和透气性好的优点。
The invention relates to the field of concrete interface agents, and particularly discloses a freeze-thaw resistant breathable concrete interface agent. The interface agent is prepared from the following raw materials in parts by weight: 50 to 100 parts of ordinary Portland cement, 10 to 20 parts of sulphoaluminate cement, 10 to 20 parts of gypsum, 10 to 20 parts of silica fume, 10 to 20 parts offly ash, 50 to 100 parts of PTB emulsion, 10 to 15 parts of waterborne acrylate laminating adhesive, 5 to 10 parts of bamboo liquefied phenolic resin, 1 to 2 parts of an air entraining agent, 1 to 2 parts of dispersant, 0.5 to 1 part of a foam breaker and 100 to 200 parts of water. The interface agent can be applied to binding new and old concrete, and has the advantages of high bonding strength,high freeze-thaw resistance and high air permeability.
本申请涉及混凝土界面剂领域,具体公开了一种抗冻融型透气混凝土界面剂。按重量份计,所述界面剂原料包括普通硅酸盐水泥50~100份,硫铝酸盐水泥10~20份,石膏10~20份,微硅粉10~20份,粉煤灰10~20份,PTB乳液50~100份,水性丙烯酸酯复膜胶10~15份,竹材液化酚醛树脂5~10份,引气剂1~2份,分散剂1~2份,消泡剂0.5~1份,水100~200份,本申请的界面剂可用于粘结新老混凝土,其具有粘结强度高、抗冻融性好和透气性好的优点。
Freeze-thaw-resistant concrete admixture and freeze-thaw-resistant concrete using same
European Patent Office | 2021
|Efficient corrosion-resistant freeze-thaw-resistant waterproof agent
European Patent Office | 2021
|Concrete freeze-thaw-resistant composite protective agent and preparation method thereof
European Patent Office | 2021
|