Antioxidant Csf/SiBCN composite material and preparation method thereof
The invention relates to the technical field of composite materials, in particular to an antioxidant Csf/SiBCN composite material and a preparation method thereof.The method comprises the steps that amorphous MA SiBCN powder, phenolic resin and an organic solvent are evenly mixed, and MA SiBCN slurry is obtained; preparing a short carbon fiber-MA SiBCN slurry layered structure system, and carrying out curing treatment to obtain a layered short carbon fiber-MA SiBCN green body; under the protection atmosphere of inert gas, the layered short carbon fiber-MA SiBCN green body is subjected to a pyrolytic reaction and cooled to the room temperature, and the porous Csf/MA SiBCN composite material is obtained; the porous Csf/MA SiBCN composite material is subjected to at least one time of dipping-crosslinking-pyrolysis treatment, and the antioxidant Csf/SiBCN composite material is obtained; the Csf/SiBCN composite material prepared by the preparation method disclosed by the invention has relatively good oxidation resistance.
本发明涉及复合材料技术领域,具体而言,涉及一种抗氧化Csf/SiBCN复合材料及其制备方法,该方法包括:将非晶MA SiBCN粉体、酚醛树脂与有机溶剂混合均匀,得到MA SiBCN浆料;制备短碳纤维‑MA SiBCN浆料层状结构体系并进行固化处理,得到层状短碳纤维‑MA SiBCN坯体;在惰性气体保护气氛下,将层状短碳纤维‑MA SiBCN坯体进行热解反应,冷却至室温,得到多孔Csf/MA SiBCN复合材料;将多孔Csf/MA SiBCN复合材料进行至少一次浸渍‑交联‑热解处理,得到抗氧化Csf/SiBCN复合材料;本发明制得的Csf/SiBCN复合材料具有较佳的抗氧化性。
Antioxidant Csf/SiBCN composite material and preparation method thereof
The invention relates to the technical field of composite materials, in particular to an antioxidant Csf/SiBCN composite material and a preparation method thereof.The method comprises the steps that amorphous MA SiBCN powder, phenolic resin and an organic solvent are evenly mixed, and MA SiBCN slurry is obtained; preparing a short carbon fiber-MA SiBCN slurry layered structure system, and carrying out curing treatment to obtain a layered short carbon fiber-MA SiBCN green body; under the protection atmosphere of inert gas, the layered short carbon fiber-MA SiBCN green body is subjected to a pyrolytic reaction and cooled to the room temperature, and the porous Csf/MA SiBCN composite material is obtained; the porous Csf/MA SiBCN composite material is subjected to at least one time of dipping-crosslinking-pyrolysis treatment, and the antioxidant Csf/SiBCN composite material is obtained; the Csf/SiBCN composite material prepared by the preparation method disclosed by the invention has relatively good oxidation resistance.
本发明涉及复合材料技术领域,具体而言,涉及一种抗氧化Csf/SiBCN复合材料及其制备方法,该方法包括:将非晶MA SiBCN粉体、酚醛树脂与有机溶剂混合均匀,得到MA SiBCN浆料;制备短碳纤维‑MA SiBCN浆料层状结构体系并进行固化处理,得到层状短碳纤维‑MA SiBCN坯体;在惰性气体保护气氛下,将层状短碳纤维‑MA SiBCN坯体进行热解反应,冷却至室温,得到多孔Csf/MA SiBCN复合材料;将多孔Csf/MA SiBCN复合材料进行至少一次浸渍‑交联‑热解处理,得到抗氧化Csf/SiBCN复合材料;本发明制得的Csf/SiBCN复合材料具有较佳的抗氧化性。
Antioxidant Csf/SiBCN composite material and preparation method thereof
一种抗氧化Csf/SiBCN复合材料及其制备方法
LI DAXIN (author) / DOU WENHAO (author) / WANG BINGZHU (author) / YANG ZHIHUA (author) / JIA DECHANG (author) / ZHOU YU (author)
2023-12-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Cf-SiBCN ceramic-based composite material and preparation method thereof
European Patent Office | 2024
|In-situ synthesized SiBCN/graphene composite material and preparation method thereof
European Patent Office | 2024
|SiBCN/SiO2 composite ceramic material as well as preparation method and application thereof
European Patent Office | 2024
|Modified SiBCN ceramic composite material as well as preparation method and application thereof
European Patent Office | 2023
|