Preparation method and application of building product of alkali-activated solid waste consolidated carbon dioxide
The invention relates to the technical field of building products prepared from solid waste, and discloses a preparation method of a building product of alkali-activated solid waste consolidated carbon dioxide, and the preparation method comprises the following steps: step 1, mixing fly ash as a main raw material with steel slag to prepare a mixture; 2, adding an alkaline activator into the mixture obtained in the step 1, and mixing to obtain slurry; 3, putting the slurry obtained in the step 2 into a mold, and pressing to form a green body; and 4, carbonizing the molded green body obtained in the step 3 to obtain the building product. The preparation method of the building product with alkali-activated solid waste consolidated carbon dioxide has the advantages of high carbon sequestration efficiency, short carbon sequestration time, low energy consumption and high compressive strength of the product.
本发明涉及固废制备建筑制品技术领域,且公开了碱激发固废固结二氧化碳的建筑制品的制备方法,包括如下步骤:步骤一:将粉煤灰作为主要原料与钢渣混合制成混合物;步骤二:在步骤一得到的混合物中加入碱性激发剂混合得到浆料;步骤三:将步骤二得到的浆料置入模具中,压制成型坯体;步骤四:将步骤三得到的成型坯体经碳化后得到所述建筑制品。该碱激发固废固结二氧化碳的建筑制品的制备方法,具备固碳效率高、固碳时间短、能耗低和产品抗压强度高的优点。
Preparation method and application of building product of alkali-activated solid waste consolidated carbon dioxide
The invention relates to the technical field of building products prepared from solid waste, and discloses a preparation method of a building product of alkali-activated solid waste consolidated carbon dioxide, and the preparation method comprises the following steps: step 1, mixing fly ash as a main raw material with steel slag to prepare a mixture; 2, adding an alkaline activator into the mixture obtained in the step 1, and mixing to obtain slurry; 3, putting the slurry obtained in the step 2 into a mold, and pressing to form a green body; and 4, carbonizing the molded green body obtained in the step 3 to obtain the building product. The preparation method of the building product with alkali-activated solid waste consolidated carbon dioxide has the advantages of high carbon sequestration efficiency, short carbon sequestration time, low energy consumption and high compressive strength of the product.
本发明涉及固废制备建筑制品技术领域,且公开了碱激发固废固结二氧化碳的建筑制品的制备方法,包括如下步骤:步骤一:将粉煤灰作为主要原料与钢渣混合制成混合物;步骤二:在步骤一得到的混合物中加入碱性激发剂混合得到浆料;步骤三:将步骤二得到的浆料置入模具中,压制成型坯体;步骤四:将步骤三得到的成型坯体经碳化后得到所述建筑制品。该碱激发固废固结二氧化碳的建筑制品的制备方法,具备固碳效率高、固碳时间短、能耗低和产品抗压强度高的优点。
Preparation method and application of building product of alkali-activated solid waste consolidated carbon dioxide
碱激发固废固结二氧化碳的建筑制品的制备方法及用途
LU HAO (author) / LIU HUACHEN (author) / ZHENG CHUANXIAO (author) / ZHAO WENJUN (author)
2024-05-17
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Preparation method of building product of coal ash-based foam material consolidated carbon dioxide
European Patent Office | 2024
|European Patent Office | 2021
|European Patent Office | 2020
|All-solid-waste alkali-activated concrete and preparation method thereof
European Patent Office | 2020
|Alkali-activated steel solid waste-based low-carbon concrete material and preparation method thereof
European Patent Office | 2024
|