High-strength ceramic tile and preparation method thereof
The invention relates to the technical field of ceramic tiles, and particularly discloses a high-strength ceramic tile and a preparation method thereof. The high-strength ceramic tile is mainly prepared from the following raw materials in parts by weight: 20-30 parts of albite, 15-25 parts of potassium feldspar, 10-20 parts of coal gangue, 2-8 parts of dolomite, 10-20 parts of kaolin, 5-15 parts of bentonite, 3-5 parts of superfine silicon powder, 3-5 parts of superfine titanium dioxide, 1-3 parts of modified pre-oxidized fiber and 0.2-0.8 part of a dispersing agent. The modified pre-oxidized fiber is obtained by grafting the pre-oxidized fiber with acetoxy propyl trimethoxy silane and tetraethylenepentamine. The ceramic tile has the characteristics of high breaking strength, high fracture modulus and high wear resistance, shows good comprehensive performance and meets market requirements.
本申请涉及瓷砖技术领域,具体公开了一种高强度瓷砖及其制备方法。高强度瓷砖主要由以下重量份的原料制成:钠长石20‑30份、钾长石15‑25份、煤矸石10‑20份、白云石2‑8份、高岭土10‑20份、膨润土5‑15份、超细硅粉3‑5份、超细钛白粉3‑5份、改性预氧丝纤维1‑3份、分散剂0.2‑0.8份;所述改性预氧丝纤维为乙酰氧基丙基三甲氧基硅烷、四乙烯五胺对预氧丝纤维接枝获得。该瓷砖具有破坏强度高、断裂模数高、耐磨性高的特点,表现出良好的综合性能,满足市场需求。
High-strength ceramic tile and preparation method thereof
The invention relates to the technical field of ceramic tiles, and particularly discloses a high-strength ceramic tile and a preparation method thereof. The high-strength ceramic tile is mainly prepared from the following raw materials in parts by weight: 20-30 parts of albite, 15-25 parts of potassium feldspar, 10-20 parts of coal gangue, 2-8 parts of dolomite, 10-20 parts of kaolin, 5-15 parts of bentonite, 3-5 parts of superfine silicon powder, 3-5 parts of superfine titanium dioxide, 1-3 parts of modified pre-oxidized fiber and 0.2-0.8 part of a dispersing agent. The modified pre-oxidized fiber is obtained by grafting the pre-oxidized fiber with acetoxy propyl trimethoxy silane and tetraethylenepentamine. The ceramic tile has the characteristics of high breaking strength, high fracture modulus and high wear resistance, shows good comprehensive performance and meets market requirements.
本申请涉及瓷砖技术领域,具体公开了一种高强度瓷砖及其制备方法。高强度瓷砖主要由以下重量份的原料制成:钠长石20‑30份、钾长石15‑25份、煤矸石10‑20份、白云石2‑8份、高岭土10‑20份、膨润土5‑15份、超细硅粉3‑5份、超细钛白粉3‑5份、改性预氧丝纤维1‑3份、分散剂0.2‑0.8份;所述改性预氧丝纤维为乙酰氧基丙基三甲氧基硅烷、四乙烯五胺对预氧丝纤维接枝获得。该瓷砖具有破坏强度高、断裂模数高、耐磨性高的特点,表现出良好的综合性能,满足市场需求。
High-strength ceramic tile and preparation method thereof
一种高强度瓷砖及其制备方法
LIU SHILIANG (author)
2024-05-24
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
/
D06M
Behandeln von Fasern, Fäden, Garnen, Textilgut, Federn oder aus solchen Materialien hergestelltem Fasergut, soweit nicht anderweitig in Klasse D06 vorgesehen
,
TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
High-strength ceramic tile and preparation method thereof
European Patent Office | 2020
|High-strength ceramic tile adhesive and preparation method thereof
European Patent Office | 2022
|High-strength ceramic glazed tile and preparation method thereof
European Patent Office | 2020
|High-strength secondary distribution ceramic tile and preparation method thereof
European Patent Office | 2023
|High-strength ceramic tile adhesive and preparation process thereof
European Patent Office | 2020
|