Recycled medium temperature modified asphalt mixture from recycled waste resources
The present invention relates to a waste resource recycled recycling warm-mix modified asphalt mixture which prepares a use aggregate for an asphalt mixture by inputting a recycling aggregate and a natural aggregate, prepares a binder by mixing a polymer material-based modification additive and a warm-mix additive with asphalt in a dry or wet method, mixes the binder having warm-mix modification properties with the use aggregate to be used. The use aggregate (A1) is prepared by comprising coarse aggregate and fine aggregate as the natural aggregate, waste asphalt concrete and waste glass material as recycled aggregate, and a filling material for asphalt pavement. The modification warm-mix binder (A2) is prepared by comprising a novel material asphalt, an old material asphalt of the recycling aggregate for asphalt concrete, and a warm-mix additive based on sulfur polymer. A functional additive and waste tire micro powder are mixed in the modification warm-mix binder (A2). The modification warm-mix binder (A2) is mixed in the use aggregate (A1) to be used.
본 발명은 폐플라스틱, 폐유리, 폐아스콘, 유황부산물 등의 폐자원을 재활용한 순환 중온 개질 아스팔트 혼합물에 관한 것으로 폐유리재와 폐아스콘을 파쇄하여 된 순환골재를 자연골재와 투입하여 아스팔트 혼합물용 사용골재를 준비하고, 폐플라스틱을 파쇄하여 된 고분자 소재의 개질첨가제와, 파라핀왁스, EB왁스, 스테아린산, 오일, 소석회를 포함하여 펠렛화 된 중온첨가제를 아스팔트에 건식 또는 습식방식으로 혼합제조해서 바인더를 준비하여, 그 중온 개질성을 갖는 바인더를 사용골재에 건식 또는 습식방식으로 혼합하여 사용토록 하기 위하여, 자연골재로서, 10∼40㎜로 파쇄된 굵은 골재 30∼50중량부와, 1∼10㎜로 파쇄된 잔골재 20∼60중량부; 재활용 순환골재로서, 1∼13㎜로 파쇄된 폐아스콘 10∼50중량부와, 1∼5㎜로 파쇄된 폐유리재 10∼40중량부; 상기 폐유리재는 투명 재질의 것이 사용되며, 아스팔트 포장용 채움재 2∼10중량부;를 포함하여 사용골재(A1)를 준비하고, 신재 아스팔트 2.3∼4.0중량부와, 아스콘용 순환골재의 구재 아스팔트 2.0∼3.0중량부에, 석유 정제과정에서 발생되는 유황폴리머로 된 중온첨가제 2.3∼3.0중량부;를 포함하여 개질 중온 바인더(A2)를 준비하고, 80∼100℃의 저융점을 갖는 0.1∼1㎜ 파쇄된 폐플라스틱재로 형성되는 고분자 소재의 개질첨가제는 아스팔트 혼합물 중량 대비 2.0∼8.0중량부; 상기 폐플라스틱은 아스팔트를 포함한 바인더와 접착력이 증대되도록 하기 위해 파쇄된 폐플라스틱의 비표면적을 보다 넓게 확보되도록 표면에 스크래치를 형성하고, 상기 폐플라스틱재는 저밀도 폴레에틸렌 재생재료가 사용되며, 상기 개질 중온 바이더(A2)에 산화방지제, 노화방지제, 제올라이트, 프로세스 오일 중 어느 하나 이상으로 된 기능성 첨가제와, 노화물성을 개질한 폐타이어 미세분말(CRM)을 더 혼합하여 구성되며, 상기 폐타이어 미세분말(CRM)은 차량용 폐타이어를 재생한 1㎜ 이하의 생고무 미분말로 형성되고, 상기 개질 중온 바이더(A2)를 사용골재(A1)에 혼합 사용토록 이루어지는 것을 특징으로 한다.
Recycled medium temperature modified asphalt mixture from recycled waste resources
The present invention relates to a waste resource recycled recycling warm-mix modified asphalt mixture which prepares a use aggregate for an asphalt mixture by inputting a recycling aggregate and a natural aggregate, prepares a binder by mixing a polymer material-based modification additive and a warm-mix additive with asphalt in a dry or wet method, mixes the binder having warm-mix modification properties with the use aggregate to be used. The use aggregate (A1) is prepared by comprising coarse aggregate and fine aggregate as the natural aggregate, waste asphalt concrete and waste glass material as recycled aggregate, and a filling material for asphalt pavement. The modification warm-mix binder (A2) is prepared by comprising a novel material asphalt, an old material asphalt of the recycling aggregate for asphalt concrete, and a warm-mix additive based on sulfur polymer. A functional additive and waste tire micro powder are mixed in the modification warm-mix binder (A2). The modification warm-mix binder (A2) is mixed in the use aggregate (A1) to be used.
본 발명은 폐플라스틱, 폐유리, 폐아스콘, 유황부산물 등의 폐자원을 재활용한 순환 중온 개질 아스팔트 혼합물에 관한 것으로 폐유리재와 폐아스콘을 파쇄하여 된 순환골재를 자연골재와 투입하여 아스팔트 혼합물용 사용골재를 준비하고, 폐플라스틱을 파쇄하여 된 고분자 소재의 개질첨가제와, 파라핀왁스, EB왁스, 스테아린산, 오일, 소석회를 포함하여 펠렛화 된 중온첨가제를 아스팔트에 건식 또는 습식방식으로 혼합제조해서 바인더를 준비하여, 그 중온 개질성을 갖는 바인더를 사용골재에 건식 또는 습식방식으로 혼합하여 사용토록 하기 위하여, 자연골재로서, 10∼40㎜로 파쇄된 굵은 골재 30∼50중량부와, 1∼10㎜로 파쇄된 잔골재 20∼60중량부; 재활용 순환골재로서, 1∼13㎜로 파쇄된 폐아스콘 10∼50중량부와, 1∼5㎜로 파쇄된 폐유리재 10∼40중량부; 상기 폐유리재는 투명 재질의 것이 사용되며, 아스팔트 포장용 채움재 2∼10중량부;를 포함하여 사용골재(A1)를 준비하고, 신재 아스팔트 2.3∼4.0중량부와, 아스콘용 순환골재의 구재 아스팔트 2.0∼3.0중량부에, 석유 정제과정에서 발생되는 유황폴리머로 된 중온첨가제 2.3∼3.0중량부;를 포함하여 개질 중온 바인더(A2)를 준비하고, 80∼100℃의 저융점을 갖는 0.1∼1㎜ 파쇄된 폐플라스틱재로 형성되는 고분자 소재의 개질첨가제는 아스팔트 혼합물 중량 대비 2.0∼8.0중량부; 상기 폐플라스틱은 아스팔트를 포함한 바인더와 접착력이 증대되도록 하기 위해 파쇄된 폐플라스틱의 비표면적을 보다 넓게 확보되도록 표면에 스크래치를 형성하고, 상기 폐플라스틱재는 저밀도 폴레에틸렌 재생재료가 사용되며, 상기 개질 중온 바이더(A2)에 산화방지제, 노화방지제, 제올라이트, 프로세스 오일 중 어느 하나 이상으로 된 기능성 첨가제와, 노화물성을 개질한 폐타이어 미세분말(CRM)을 더 혼합하여 구성되며, 상기 폐타이어 미세분말(CRM)은 차량용 폐타이어를 재생한 1㎜ 이하의 생고무 미분말로 형성되고, 상기 개질 중온 바이더(A2)를 사용골재(A1)에 혼합 사용토록 이루어지는 것을 특징으로 한다.
Recycled medium temperature modified asphalt mixture from recycled waste resources
폐자원을 재활용한 순환 중온 개질 아스팔트 혼합물
JO YOUNG JIN (author) / JU JI HONG (author) / LEE SANG CHEOL (author)
2021-10-01
Patent
Electronic Resource
Korean
RECYCLED ASPHALT MIXTURE MANUFACTURING METHOD AND RECYCLED ASPHALT MIXTURE
European Patent Office | 2020
|European Patent Office | 2024
|RECYCLED ASPHALT MIXTURE PRODUCTION METHOD AND RECYCLED ASPHALT MIXTURE PRODUCTION DEVICE
European Patent Office | 2021
|