METHOD FOR RAPID REPAIRMENT OF RAILWAY SLOPES
The present invention relates to a method for reinforcing and repairing a railway embankment. The method for reinforcing and repairing a railway embankment according to the present invention comprises: a step (a) of installing holders on a damaged railway embankment; a step (b) of installing composite mats, each of which includes an upper sheet having permeability, a lower sheet coupled to the underside of the upper sheet, and a powder-state ultra-rapid binder filled between the upper sheet and the lower sheet, on the holders; a step (c) of supplying water through the upper sheet of the composite mat to harden the ultra-rapid binder; and a step (d) of filling spaces between the holders and the composite mats with a low-flow fill material and hardening the low-flow fill material, wherein the low-flow fill material consists of 90 to 92 wt% of a filler containing fly ash and steel slag, and 8 to 10 wt% of a binding agent consisting of 85 to 90 wt% of a calcium aluminate material, 3 to 5 wt% of cement, and 5 to 10 wt% of a calcium sulphoaluminate material. The low-flow fill material is additionally mixed with a liquid thickening agent in a state mixed with water. Therefore, the method for reinforcing and repairing a railway embankment can prevent the loss of fill material on an embankment using the low-flow fill material.
본 발명은 철도 사면 보수보강 공법에 관한 것이다. 본 발명에 따른 철도 사면 보수보강 공법은 (a)손상된 철도 사면에 거치대를 설치하는 단계 (b)투수성을 가지는 상부시트와 상부시트의 하부에 결합되는 하부시트 및 상부시트 및 하부시트 사이에 충진되는 분말 상태의 초속경 바인더를 구비하는 복합매트를 거치대에 설치하는 단계 (c)복합매트의 상부시트를 통해 물을 공급하여 초속경 바인더를 경화시키는 단계; 및 (d)거치대와 복합매트 사이의 공간에 저유동 채움재를 충진하여 경화시키는 단계를 구비하며, 저유동 채움재는 플라이애쉬와 제강슬래그를 포함하는 필러 90~92 중량%와, 칼슘알루미네이트계 물질 85~90중량%, 시멘트 3~5%, 칼슘설포알루미네이트계 물질 5~10중량%로 이루어지는 결합재 8~10 중량%로 이루어지며, 저유동 채움재는 물과 혼합된 상태에서 액상 증점제가 추가적으로 배합되는 것에 특징이 있다.
METHOD FOR RAPID REPAIRMENT OF RAILWAY SLOPES
The present invention relates to a method for reinforcing and repairing a railway embankment. The method for reinforcing and repairing a railway embankment according to the present invention comprises: a step (a) of installing holders on a damaged railway embankment; a step (b) of installing composite mats, each of which includes an upper sheet having permeability, a lower sheet coupled to the underside of the upper sheet, and a powder-state ultra-rapid binder filled between the upper sheet and the lower sheet, on the holders; a step (c) of supplying water through the upper sheet of the composite mat to harden the ultra-rapid binder; and a step (d) of filling spaces between the holders and the composite mats with a low-flow fill material and hardening the low-flow fill material, wherein the low-flow fill material consists of 90 to 92 wt% of a filler containing fly ash and steel slag, and 8 to 10 wt% of a binding agent consisting of 85 to 90 wt% of a calcium aluminate material, 3 to 5 wt% of cement, and 5 to 10 wt% of a calcium sulphoaluminate material. The low-flow fill material is additionally mixed with a liquid thickening agent in a state mixed with water. Therefore, the method for reinforcing and repairing a railway embankment can prevent the loss of fill material on an embankment using the low-flow fill material.
본 발명은 철도 사면 보수보강 공법에 관한 것이다. 본 발명에 따른 철도 사면 보수보강 공법은 (a)손상된 철도 사면에 거치대를 설치하는 단계 (b)투수성을 가지는 상부시트와 상부시트의 하부에 결합되는 하부시트 및 상부시트 및 하부시트 사이에 충진되는 분말 상태의 초속경 바인더를 구비하는 복합매트를 거치대에 설치하는 단계 (c)복합매트의 상부시트를 통해 물을 공급하여 초속경 바인더를 경화시키는 단계; 및 (d)거치대와 복합매트 사이의 공간에 저유동 채움재를 충진하여 경화시키는 단계를 구비하며, 저유동 채움재는 플라이애쉬와 제강슬래그를 포함하는 필러 90~92 중량%와, 칼슘알루미네이트계 물질 85~90중량%, 시멘트 3~5%, 칼슘설포알루미네이트계 물질 5~10중량%로 이루어지는 결합재 8~10 중량%로 이루어지며, 저유동 채움재는 물과 혼합된 상태에서 액상 증점제가 추가적으로 배합되는 것에 특징이 있다.
METHOD FOR RAPID REPAIRMENT OF RAILWAY SLOPES
철도 사면 보수보강 공법
RYU YONG SUN (author) / HAN JIN GYU (author)
2023-05-25
Patent
Electronic Resource
Korean
METHOD FOR RAPID REPAIRMENT OF RAILWAY SLOPES USING CEMENTIOUS COMPOSITE MAT
European Patent Office | 2024
|