METHODS FOR CALCINING GYPSUM
A method for calcining gypsum includes subjecting a composition including gypsum dihydrate to a predetermined vacuum. The method further includes maintaining the composition under the at least partial vacuum at a calcining temperature for a predetermined calcining time. The calcining temperature may be in a range from 60°C to 125 °C, or in a range from 65 °C to 85°C. The vacuum may be in a range from 25 mbar to 50 mbar. The predetermined calcining time may be in a range from 3 hours to 10 hours. The maintaining is effective to at least partially remove water of crystallization from the gypsum dihydrate to convert the composition to a product including gypsum hemihydrate.
Un procédé de calcination de gypse consiste à soumettre une composition comprenant du dihydrate de gypse à un vide prédéterminé. Le procédé consiste en outre à maintenir la composition sous le vide au moins partiel à une température de calcination pendant un temps de calcination prédéterminé. La température de calcination peut être dans une plage de 60 °C à 125 °C, ou dans une plage de 65 °C à 85 °C ; le vide peut être dans une plage de 25 mbar à 50 mbar. Le temps de calcination prédéterminé peut être dans une plage de 3 heures à 10 heures. Le maintien est efficace pour éliminer au moins partiellement l'eau de cristallisation du dihydrate de gypse afin de convertir la composition en un produit comprenant du gypse hémihydraté.
METHODS FOR CALCINING GYPSUM
A method for calcining gypsum includes subjecting a composition including gypsum dihydrate to a predetermined vacuum. The method further includes maintaining the composition under the at least partial vacuum at a calcining temperature for a predetermined calcining time. The calcining temperature may be in a range from 60°C to 125 °C, or in a range from 65 °C to 85°C. The vacuum may be in a range from 25 mbar to 50 mbar. The predetermined calcining time may be in a range from 3 hours to 10 hours. The maintaining is effective to at least partially remove water of crystallization from the gypsum dihydrate to convert the composition to a product including gypsum hemihydrate.
Un procédé de calcination de gypse consiste à soumettre une composition comprenant du dihydrate de gypse à un vide prédéterminé. Le procédé consiste en outre à maintenir la composition sous le vide au moins partiel à une température de calcination pendant un temps de calcination prédéterminé. La température de calcination peut être dans une plage de 60 °C à 125 °C, ou dans une plage de 65 °C à 85 °C ; le vide peut être dans une plage de 25 mbar à 50 mbar. Le temps de calcination prédéterminé peut être dans une plage de 3 heures à 10 heures. Le maintien est efficace pour éliminer au moins partiellement l'eau de cristallisation du dihydrate de gypse afin de convertir la composition en un produit comprenant du gypse hémihydraté.
METHODS FOR CALCINING GYPSUM
PROCÉDÉS DE CALCINATION DE GYPSE