Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Secondary IMC formation induced by Kirkendall voiding in Cu/Sn-3.5Ag solder joints
JOURNAL OF MATERIALS RESEARCH -PITTSBURGH THEN WARRENDALE- ; 25 ; 1854-1858
01.01.2010
5 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Heat-treatment to suppress the formation of Kirkendall voids in Sn-3.5Ag/Cu solder joints
British Library Online Contents | 2013
|Effect of deposit thickness during electroplating on Kirkendall voiding at Sn/Cu joints
British Library Online Contents | 2014
|On the root cause of Kirkendall voiding in Cu~3Sn
British Library Online Contents | 2011
|Kirkendall voids in the intermetallic layers of solder joints in MEMS
British Library Online Contents | 2009
|Effect of La addition on adhesive strength and fracture behavior of Sn-3.5Ag solder joints
British Library Online Contents | 2011
|