The present invention discloses a high-waterproof non-leakage ceramsite enhanced aerated building block which is characterized by comprising the following raw materials in parts by weight: 10-14 parts of perlite, 30-50 parts of ceramsite, 15-30 parts of fly ash, 10-15 parts of quick lime, 15-20 parts of cement, 0.3-0.5 part of aluminum powder, 2-4 parts of gypsum powder, 3-5 parts of butyl rubber, 0.3-0.5 part of lignin calcium sulfonate, 1-3 parts of iron powder, 3-5 parts of nano aluminum oxide, 2-4 parts of carbon black, 15-20 parts of absolute ethanol, and proper amount of water; the process solves the problems of being fragile and light and uneven in distribution of the ceramsite in slurry in processing process, the added butyl rubber enhances waterproof performance of the ceramsite and sound insulation of the building block, the high-waterproof non-leakage ceramsite enhanced aerated building block has stable chemical properties, excellent physical properties and other characteristics. The process is simple, efficiency is high, emissions of waste substances are avoided, the environment is not polluted, and the high-waterproof non-leakage ceramsite enhanced aerated building block has significant economic and social benefits.
High-waterproof non-leakage ceramsite enhanced aerated building block
The present invention discloses a high-waterproof non-leakage ceramsite enhanced aerated building block which is characterized by comprising the following raw materials in parts by weight: 10-14 parts of perlite, 30-50 parts of ceramsite, 15-30 parts of fly ash, 10-15 parts of quick lime, 15-20 parts of cement, 0.3-0.5 part of aluminum powder, 2-4 parts of gypsum powder, 3-5 parts of butyl rubber, 0.3-0.5 part of lignin calcium sulfonate, 1-3 parts of iron powder, 3-5 parts of nano aluminum oxide, 2-4 parts of carbon black, 15-20 parts of absolute ethanol, and proper amount of water; the process solves the problems of being fragile and light and uneven in distribution of the ceramsite in slurry in processing process, the added butyl rubber enhances waterproof performance of the ceramsite and sound insulation of the building block, the high-waterproof non-leakage ceramsite enhanced aerated building block has stable chemical properties, excellent physical properties and other characteristics. The process is simple, efficiency is high, emissions of waste substances are avoided, the environment is not polluted, and the high-waterproof non-leakage ceramsite enhanced aerated building block has significant economic and social benefits.
High-waterproof non-leakage ceramsite enhanced aerated building block
HUANG ERHUA (author)
2015-09-16
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Ceramsite enhanced good aging resistance aerated building block
European Patent Office | 2015
|Ceramsite enhanced low crack tendency aerated building block
European Patent Office | 2015
|European Patent Office | 2023
|Ceramsite aerated building block added with shell powder
European Patent Office | 2015
|