The present invention discloses a ceramsite enhanced good aging resistance aerated building block which is characterized by comprising the following raw materials in parts by weight: 8-12 parts of silica, 30-50 parts of ceramsite, 15-30 parts of fly ash, 10-15 parts of quick lime, 15-20 parts of cement, 0.2-0.4 part of aluminum powder, 2-4 parts of silicone-modified acrylate emulsion, 2-4 parts of gypsum powder, 0.1-0.3 part of magnesium chloride, 0.3-0.5 part of calcium lignosulphonate, 1-3 parts of iron powder, 3-5 parts of nano aluminum oxide, 2-4 parts of carbon black, 15-20 parts of absolute ethanol, and proper amount of water; the process solves the problems of being fragile and light and uneven in distribution of the ceramsite in slurry in processing process, the added silicone-modified acrylate emulsion improves the aging resistance performance of the ceramsite, the added magnesium chloride enhances the early strength of the block, and the building block is not only high in strength, good in heat resistance, low in density, and also has excellent resistance to aging, and heat insulation performance.
Ceramsite enhanced good aging resistance aerated building block
The present invention discloses a ceramsite enhanced good aging resistance aerated building block which is characterized by comprising the following raw materials in parts by weight: 8-12 parts of silica, 30-50 parts of ceramsite, 15-30 parts of fly ash, 10-15 parts of quick lime, 15-20 parts of cement, 0.2-0.4 part of aluminum powder, 2-4 parts of silicone-modified acrylate emulsion, 2-4 parts of gypsum powder, 0.1-0.3 part of magnesium chloride, 0.3-0.5 part of calcium lignosulphonate, 1-3 parts of iron powder, 3-5 parts of nano aluminum oxide, 2-4 parts of carbon black, 15-20 parts of absolute ethanol, and proper amount of water; the process solves the problems of being fragile and light and uneven in distribution of the ceramsite in slurry in processing process, the added silicone-modified acrylate emulsion improves the aging resistance performance of the ceramsite, the added magnesium chloride enhances the early strength of the block, and the building block is not only high in strength, good in heat resistance, low in density, and also has excellent resistance to aging, and heat insulation performance.
Ceramsite enhanced good aging resistance aerated building block
HUANG ERHUA (author)
2015-09-16
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Ceramsite enhanced low crack tendency aerated building block
European Patent Office | 2015
|European Patent Office | 2023
|High-waterproof non-leakage ceramsite enhanced aerated building block
European Patent Office | 2015
|Ceramsite aerated building block added with shell powder
European Patent Office | 2015
|