Alkali activated phosphorus slag micropowder light foam concrete thermal insulation board and preparation method thereof
The invention discloses an alkali activated phosphorus slag micropowder light foam concrete thermal insulation board, which comprises the following components by mass: 35-39% of phosphorus slag micropowder, 6-10% of an alkali activator, 7-12% of a coagulation regulating agent, 9-15% of a modifier, 0.4-0.8% of fiber, 9-12% of a foaming agent, and 22-26% of water. According to the invention, phosphorus slag micropowder is adopted as the main cementing material, through strong alkali activation and incorporation of appropriate coagulation regulating component and modification components, the coagulation time and shrinkage performance of foam concrete are controlled. The foam concrete thermal insulation board prepared by the method provided by the invention has an absolute dry density controlled at 150-250kg/m<3>, 28d compressive strength of 0.30-0.63Mpa, a heat conductivity coefficient of 0.042-0.051W/m.K, and a water absorption rate of 5-8%, thus being an ideal exterior wall external insulation wall enclosure material.
Alkali activated phosphorus slag micropowder light foam concrete thermal insulation board and preparation method thereof
The invention discloses an alkali activated phosphorus slag micropowder light foam concrete thermal insulation board, which comprises the following components by mass: 35-39% of phosphorus slag micropowder, 6-10% of an alkali activator, 7-12% of a coagulation regulating agent, 9-15% of a modifier, 0.4-0.8% of fiber, 9-12% of a foaming agent, and 22-26% of water. According to the invention, phosphorus slag micropowder is adopted as the main cementing material, through strong alkali activation and incorporation of appropriate coagulation regulating component and modification components, the coagulation time and shrinkage performance of foam concrete are controlled. The foam concrete thermal insulation board prepared by the method provided by the invention has an absolute dry density controlled at 150-250kg/m<3>, 28d compressive strength of 0.30-0.63Mpa, a heat conductivity coefficient of 0.042-0.051W/m.K, and a water absorption rate of 5-8%, thus being an ideal exterior wall external insulation wall enclosure material.
Alkali activated phosphorus slag micropowder light foam concrete thermal insulation board and preparation method thereof
GAO YUXIN (author) / CHEN JING (author) / GAN GEJIN (author) / LU JIALIN (author) / XU FENLIAN (author)
2016-01-27
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Slag micropowder cementing material and preparation method thereof
European Patent Office | 2022
|Preparation method for phosphorus-slag micropowder applied to cement-based material
European Patent Office | 2015
|European Patent Office | 2024
|Alkali-activated slag concrete and preparation method thereof
European Patent Office | 2023
|